Find suppliers for this alloy C11025
Chemical Composition
Elements
Cu(1,2,3) Pb Zn Fe Ag As O Sb Te
(1) The following additional maximum limits shall apply: Se 10 ppm (0.0010%); Bi 5 ppm (0.0005%); Sn 150 ppm (0.0150%); Ni 150 ppm (0.0150%); S 20 ppm (0.0020%); Cd 100 ppm (0.0100%).
(2) The total maximum allowable of named elements is 750 ppm (0.0750%) not including oxygen.
(3) Cu value includes Ag.
Min (%) 99.90 0.0150 0.0100
Max (%) 0.0450 0.0080 0.0020 0.0150 0.0010 0.0400 0.0050 0.0010
Mechanical Properties

No mechanical properties for this alloy

Physical Properties

No physical properties for this alloy

Fabrication Properties

No fabrication properties for this alloy

Common Fabrication Processes

No fabrication process properties for this alloy

Thermal Properties

No thermal properties for this alloy

Typical Uses

No information for this alloy

Applicable Specifications
Form Specific Sub-Form Application System Standard Description
ASTM B224 Standard Classification of Coppers
Rod ASTM B49 HOT-ROLLED COPPER ROD REDRAW FOR ELECTRICAL PURPOSES
Corrosion Properties