Find suppliers for this alloy C11700
Chemical Composition
Elements
Cu(1,2) P B
(1) Cu value includes Ag.
(2) Includes B + P.
Min (%) 99.9 0.004
Max (%) 0.04 0.02
Mechanical Properties

No mechanical properties for this alloy

Physical Properties

No physical properties for this alloy

Fabrication Properties

No fabrication properties for this alloy

Common Fabrication Processes

No fabrication process properties for this alloy

Thermal Properties

No thermal properties for this alloy

Typical Uses

No information for this alloy

Applicable Specifications
Form Specific Sub-Form Application System Standard Description
ASTM B577 Detection of Cuperous Oxide (Hydrogen Embrittlement Susceptibility) in Copper
Brazing Filler Metal FEDERAL QQ-B-650 BRAZING ALLOY, COPPER, COPPER-ZINC, AND COPPER-PHOSPHORUS
Corrosion Properties

No Corrosion Properties Available.