Find suppliers for this alloy
C10810
| Elements | |||
|---|---|---|---|
| Cu(1) | Ca | O | |
|
(1) Cu + Sum of Named Elements 99.5% min. |
|||
| Min (%) | 99.95 | 0.001 | |
| Max (%) | 0.010 | 0.001 | |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
Elongation (%) |
Vickers Hardness, 500 gm |
|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | |||||
| Strip | 1/8 Hard | H00 |
31 Min 36 Typ 40 Max |
36 Typ |
71 Typ |
| Melting Point - Liquidus°F | 1981 |
|---|---|
| Melting Point - Solidus°F | 1981 |
| Densitylb/cu in. at 68°F | 0.323 |
| Specific Gravity | 8.94 |
| Electrical Conductivity% IACS at 68°F | 101 |
| Electrical Resistivityohm.cmil/ft at 68°F | 10.3 |
| Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F | 230 |
| Coefficient of Thermal Expansion 68-57210 to -6 power per °F (68 – 572°F) | 9.8 |
| Modulus of Elasticity in Tensionksi | 17180 |
| Poisson's Ratioksi | 0.30 |
| Technique | Suitability |
|---|---|
| Soldering | Excellent |
| Brazing | Excellent |
| Capacity for Being Cold Worked | Excellent |
| Capacity for Being Hot Formed | Excellent |
Common Fabrication Processes
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Electrical | Conductors, Electrical and Thermal, High Strength | ||
| Fasteners | Lead Frames, Connector Components | ||
| Industrial | Terminal Connectors |
Applicable Specifications