Find suppliers for this alloy
C10920
| Elements | ||
|---|---|---|
| Cu(1) | O | |
|
(1) Cu value includes Ag. |
||
| Min (%) | 99.90 | |
| Max (%) | 0.02 | |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
| Form | Specific Sub-Form | Application | System | Standard | Description |
|---|---|---|---|---|---|
| Brazing Filler Metal | FEDERAL | QQ-B-650 | BRAZING ALLOY, COPPER, COPPER-ZINC, AND COPPER-PHOSPHORUS | ||
| Bus Bar, Rod and Shapes, General Purpose, same | ASME | SB187 | COPPER BUS BAR, ROD AND SHAPES AND GENERAL PURPOSE ROD, BAR AND SHAPES | ||
| ASTM | B187/B187M | COPPER BUS BAR, ROD AND SHAPES AND GENERAL PURPOSE ROD, BAR AND SHAPES |
Corrosion Properties