Find suppliers for this alloy
C10930
| Elements | |||
|---|---|---|---|
| Cu(1) | Ag(2) | O | |
|
(1) Cu value includes Ag. (2) Ag 0.044% min is the equivelant of, Ag 13 Troy Oz min. |
|||
| Min (%) | 99.90 | 0.044 | |
| Max (%) | 0.02 | ||
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Electrical | Busbars | Conductivity (Electrical) | Electrical Conductivity |
| Busbars | Conductivity (Thermal) | Thermal Conductivity | |
| Busbars | Corrosion Resistance | Corrosion Resistance | |
| Busbars | Softening Resistance | Resistance to Softening |
| Form | Specific Sub-Form | Application | System | Standard | Description |
|---|---|---|---|---|---|
| Bar | ASTM | B187/B187M | COPPER BUS BAR, ROD AND SHAPES AND GENERAL PURPOSE ROD, BAR AND SHAPES | ||
| Brazing Filler Metal | FEDERAL | QQ-B-650 | BRAZING ALLOY, COPPER, COPPER-ZINC, AND COPPER-PHOSPHORUS | ||
| Bus Bar, Rod and Shapes, General Purpose, same | ASME | SB187 | COPPER BUS BAR, ROD AND SHAPES AND GENERAL PURPOSE ROD, BAR AND SHAPES | ||
| Shapes | ASTM | B187/B187M | COPPER BUS BAR, ROD AND SHAPES AND GENERAL PURPOSE ROD, BAR AND SHAPES |
Corrosion Properties