Find suppliers for this alloy
C11020
| Elements | |
|---|---|
| Cu(1,2,3) | |
|
(1) This is a high conductivity copper which has, in the annealed condition a minimum conductivity of 100% IACS. (2) Oxygen and trace elements may vary depending on the process. (3) Cu value includes Ag. |
|
| Min (%) | 99.90 |
| Max (%) | |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Architecture | Downspouts | Appearance | Appearance |
| Downspouts | Corrosion Resistance | Corrosion Resistance | |
| Downspouts | Solderability | Solderability | |
| Flashing | Appearance | Appearance | |
| Flashing | Corrosion Resistance | Corrosion Resistance | |
| Roofing | Appearance | Appearance | |
| Roofing | Corrosion Resistance | Corrosion Resistance | |
| Roofing | Solderability | Solderability | |
| Skylight Frames | Appearance | Appearance | |
| Skylight Frames | Corrosion Resistance | Corrosion Resistance | |
| Building | Wire Screening | Appearance | Appearance |
| Wire Screening | Corrosion Resistance | Corrosion Resistance | |
| Wire Screening | Forming Characteristics | Formability | |
| Electrical | Busbars | Conductivity (Electrical) | Electrical Conductivity |
| Busbars | Conductivity (Thermal) | Thermal Conductivity | |
| Busbars | Corrosion Resistance | Corrosion Resistance | |
| Lead Frames | Conductivity (Electrical) | Electrical Conductivity | |
| Lead Frames | Conductivity (Thermal) | Thermal Conductivity | |
| Panel Boards | Conductivity (Electrical) | Electrical Conductivity | |
| Panel Boards | Conductivity (Thermal) | Thermal Conductivity | |
| Panel Boards | Corrosion Resistance | Corrosion Resistance | |
| Terminal Connectors | Conductivity (Electrical) | Electrical Conductivity | |
| Terminal Connectors | Conductivity (Thermal) | Thermal Conductivity | |
| Terminal Connectors | Corrosion Resistance | Corrosion Resistance | |
| Fasteners | Fasteners | Appearance | Appearance |
| Fasteners | Conductivity (Electrical) | Electrical Conductivity | |
| Fasteners | Corrosion Resistance | Corrosion Resistance | |
| Industrial | Chemical Process Equipment | Corrosion Resistance | Corrosion Resistance |
| Chemical Process Equipment | Corrosion Resistance | Corrosion Resistance to Acids | |
| Chemical Process Equipment | Corrosion Resistance | Corrosion Resistance to Non Oxidizing Acids | |
| Chimney Cap Screens | Appearance | Appearance | |
| Chimney Cap Screens | Corrosion Resistance | Corrosion Resistance | |
| Chlorine Cells | Corrosion Resistance | Corrosion Resistance | |
| Chlorine Cells | Forming Characteristics | Formability | |
| Pressure Vessels | Conductivity (Thermal) | Thermal Conductivity | |
| Pressure Vessels | Corrosion Resistance | Corrosion Resistance | |
| Pressure Vessels | Mechanical Properties | Moderate Strength | |
| Printing Rolls | Conductivity (Electrical) | Electrical Conductivity | |
| Printing Rolls | Conductivity (Thermal) | Thermal Conductivity | |
| Printing Rolls | Corrosion Resistance | Corrosion Resistance |
Applicable Specifications
Corrosion Properties