Find suppliers for this alloy
C11025
| Elements | |||||||||
|---|---|---|---|---|---|---|---|---|---|
| Cu(1,2,3) | Pb | Zn | Fe | Ag | As | O | Sb | Te | |
|
(1) The following additional maximum limits shall apply: Se 10 ppm (0.0010%); Bi 5 ppm (0.0005%); Sn 150 ppm (0.0150%); Ni 150 ppm (0.0150%); S 20 ppm (0.0020%); Cd 100 ppm (0.0100%). (2) The total maximum allowable of named elements is 750 ppm (0.0750%) not including oxygen. (3) Cu value includes Ag. |
|||||||||
| Min (%) | 99.90 | 0.0150 | 0.0100 | ||||||
| Max (%) | 0.0450 | 0.0080 | 0.0020 | 0.0150 | 0.0010 | 0.0400 | 0.0050 | 0.0010 | |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
| Form | Specific Sub-Form | Application | System | Standard | Description |
|---|---|---|---|---|---|
| ASTM | B224 | Standard Classification of Coppers | |||
| Rod | ASTM | B49 | HOT-ROLLED COPPER ROD REDRAW FOR ELECTRICAL PURPOSES |
Corrosion Properties