SSL certificate problem: certificate has expired
Find suppliers for this alloy C11040
Chemical Composition
Elements
Cu(1,2,3) Pb Fe Ag As O Sb Te
(1) Cu value is exclusive of Ag
(2) The following additional maximum limits shall apply: Se 2ppm (0.0002%); Bi 1.0ppm (0.00010%); Group Total Te + Se +Bi 3ppm(0.0003%); Sn 5ppm (0.0005%); Ni 10ppm (0.0010%); S 15ppm (0.0015%). The total maximum allowable of named elements is 65 ppm (0.0065%) - does not include oxygen.
(3) This is a high conductivity copper which has, in the annealed condition a minimum conductivity of 100% IACS.
Min (%) 99.90 0.0100
Max (%) 0.0005 0.0010 0.0025 0.0005 0.0650 0.0004 0.0002
Mechanical Properties

No mechanical properties for this alloy

Physical Properties

No physical properties for this alloy

Fabrication Properties

No fabrication properties for this alloy

Common Fabrication Processes

No fabrication process properties for this alloy

Thermal Properties

No thermal properties for this alloy

Typical Uses

No information for this alloy

Applicable Specifications
Form Specific Sub-Form Application System Standard Description
ASTM B224 Standard Classification of Coppers
Rod ASTM B49 HOT-ROLLED COPPER ROD REDRAW FOR ELECTRICAL PURPOSES
Strip ASTM B272 COPPER FLAT PRODUCTS WITH FINISHED (ROLLED OR DRAWN) EDGES (FLAT WIRE AND STRIP)
Wire ASTM B272 COPPER FLAT PRODUCTS WITH FINISHED (ROLLED OR DRAWN) EDGES (FLAT WIRE AND STRIP)
Corrosion Properties

No Corrosion Properties Available.