Find suppliers for this alloyC11040
Chemical Composition
Element
Cu(1,2,3)PbFeAgAsOSbTe
(1) Cu value is exclusive of Ag (2) The following additional maximum limits shall apply: Se 2ppm (0.0002%); Bi 1.0ppm (0.00010%); Group Total Te + Se +Bi 3ppm(0.0003%); Sn 5ppm (0.0005%); Ni 10ppm (0.0010%); S 15ppm (0.0015%). The total maximum allowable of named elements is 65 ppm (0.0065%) - does not include oxygen. (3) This is a high conductivity copper which has, in the annealed condition a minimum conductivity of 100% IACS.
Min (%)99.900.0100
Max (%)0.00050.00100.00250.00050.06500.00040.0002
Mechanical Properties

No mechanical properties for this alloy

Physical Properties

No physical properties for this alloy

Fabrication Properties

No fabrication properties for this alloy

Fabrication Process Properties

No fabrication process properties for this alloy

Thermal Characteristics

No thermal characteristics for this alloy

Typical Uses

No information available.

Applicable Specifications
Form Specific Sub-Form System Standard Description
ASTMB224Standard Classification of Coppers
RodASTMB49HOT-ROLLED COPPER ROD REDRAW FOR ELECTRICAL PURPOSES
StripASTMB272COPPER FLAT PRODUCTS WITH FINISHED (ROLLED OR DRAWN) EDGES (FLAT WIRE AND STRIP)
WireFlatASTMB272COPPER FLAT PRODUCTS WITH FINISHED (ROLLED OR DRAWN) EDGES (FLAT WIRE AND STRIP)
Corrosion Properties

No information available.