Find suppliers for this alloyC11045
Chemical Composition
Element
Cu(1,2)PbFeAgAsOSbTe
(1) These total maximum limits shall apply; Se 2ppm(0.0002%); Bi 0.5ppm (0.00005%); Sn 5 ppm (0.0005%); Ni 10ppm (0.0010%); S 15 ppm (0.0015%). (2) Cu value includes Ag.
Min (%)99.900.0100
Max (%)0.00050.00100.00250.00050.06500.00040.0002
Mechanical Properties

No mechanical properties for this alloy

Physical Properties

No physical properties for this alloy

Fabrication Properties

No fabrication properties for this alloy

Fabrication Process Properties

No fabrication process properties for this alloy

Thermal Characteristics

No thermal characteristics for this alloy

Typical Uses

No information available.

Applicable Specifications

No applicable specifications for this alloy

Corrosion Properties

No information available.