| Elements | ||||||||
|---|---|---|---|---|---|---|---|---|
| Cu(1) | Pb | Fe | Ag | As | O | Sb | Te | |
|
(1) The following additional impurity maximum limits shall apply: Bi 1 ppm (0.0015%); Ni 15 ppm (0.0015%); S 15 ppm (0.0015%); Se 2 ppm (0.0002%); Sn 15 ppm (0.0015%); |
||||||||
| Min (%) | 99.90 | 0.0100 | ||||||
| Max (%) | 0.0005 | 0.0030 | 0.0025 | 0.0005 | 0.0650 | 0.0004 | 0.0002 | |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Typical Uses
Applicable Specifications
Corrosion Properties