Find suppliers for this alloy C12600
Chemical Composition
Elements
Cu(1) P
(1) Cu value includes Ag.
Min (%) 99.5 0.20
Max (%) 0.40
Mechanical Properties *
Form Temper Temper Code Tensile Strength
(ksi)
YS-0.2% Offset
(ksi)
Elongation
(%)
Vickers Hardness, 3000 gm
* Measured at room temperature, 68°F (20°C).
Flat Products Annealed O61 36 Min
38 Typ
41 Max
8 Min
10 Typ
12 Max
50 Min
56 Typ
Physical Properties
Melting Point - Liquidus°F 1980
Densitylb/cu in. at 68°F 0.321
Specific Gravity 8.89
Electrical Conductivity% IACS at 68°F 29
Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F 77.4
Coefficient of Thermal Expansion 68-57210 to -6 power per °F (68 – 572°F) 10.3
Modulus of Elasticity in Tensionksi 14800
Modulus of Rigidityksi 8100
Fabrication Properties

No fabrication properties for this alloy

Common Fabrication Processes

No fabrication process properties for this alloy

Thermal Properties

No thermal properties for this alloy

Typical uses
Product Category Product Reason Category Reason
Consumer Refrigerators
Industrial AC-R Heat Eexchanger Tubing
Heat Exchanger Components
Applicable Specifications

No applicable specifications for this alloy

Corrosion Properties

No Corrosion Properties Available.