Find suppliers for this alloyC12600
Chemical Composition
Element
Cu(1)P
(1) Cu value includes Ag.
Min (%)99.50.20
Max (%)0.40
Mechanical Properties*
Form
Temper
Temper Code
Tensile Strength
(ksi)
YS-0.2% Offset
Elongation
(%)
Vickers Hardness, 3000 gm
Flat ProductsAnnealedO6136   Min
38   Typ
41   Max
8   Min
10   Typ
12   Max
50   Min
56   Typ
* Measured at room temperature, 68°F (20°C).
Physical Properties
Melting Point - Liquidus°F1980
Densitylb/cu in. at 68°F0.321
Specific Gravity8.89
Electrical Conductivity% IACS at 68°F29
Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F77.4
Coefficient of Thermal Expansion 68-57210⁻⁶ per °F (68 – 572°F)10.3
Modulus of Elasticity in Tensionksi14800
Modulus of Rigidityksi8100
Fabrication Properties
Technique Suitability
BrazingExcellent
Fabrication Process Properties

No fabrication process properties for this alloy

Thermal Characteristics

No thermal characteristics for this alloy

Typical uses
Product Category Product Reason Category Reason
ConsumerRefrigerators
IndustrialAC-R Heat Eexchanger Tubing
Heat Exchanger Components
Applicable Specifications

No applicable specifications for this alloy

Corrosion Properties

No information available.