C13500
| Elements | |||
|---|---|---|---|
| Cu(1) | P | Ag(2) | |
|
(1) Cu value includes Ag. (2) Ag 0.034% min is the equivelant of, Ag 10 Troy Oz min. |
|||
| Min (%) | 99.99 | 0.034 | |
| Max (%) | 0.0005 | ||