Find suppliers for this alloy
C14400
| Elements | ||||||||
|---|---|---|---|---|---|---|---|---|
| Cu(1) | Sn | Zn | Fe | P | Ni | Sb | Te | |
|
(1) Cu value includes Ag. |
||||||||
| Min (%) | 99.90 | 0.10 | 0.013 | |||||
| Max (%) | 0.20 | 0.05 | 0.03 | 0.025 | 0.05 | 0.003 | 0.02 | |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
| Form | Specific Sub-Form | Application | System | Standard | Description |
|---|---|---|---|---|---|
| Brazing Filler Metal | FEDERAL | QQ-B-650 | BRAZING ALLOY, COPPER, COPPER-ZINC, AND COPPER-PHOSPHORUS |
Corrosion Properties