Find suppliers for this alloyC14400
Chemical Composition
Element
Cu(1)SnZnFePNiSbTe
(1) Cu value includes Ag.
Min (%)99.900.100.013
Max (%)0.200.050.030.0250.050.0030.02
Mechanical Properties

No mechanical properties for this alloy

Physical Properties

No physical properties for this alloy

Fabrication Properties

No fabrication properties for this alloy

Fabrication Process Properties

No fabrication process properties for this alloy

Thermal Characteristics

No thermal characteristics for this alloy

Typical Uses

No information available.

Applicable Specifications
Form System Standard Description
Brazing Filler MetalFEDERALQQ-B-650BRAZING ALLOY, COPPER, COPPER-ZINC, AND COPPER-PHOSPHORUS
Corrosion Properties

No information available.