Find suppliers for this alloy
C14410
| Elements | |||||
|---|---|---|---|---|---|
| Cu(1,2) | Pb | Sn | Fe | P | |
|
(1) Includes Cu + Ag + Sn. (2) Cu value includes Ag. |
|||||
| Min (%) | 99.90 | 0.10 | 0.005 | ||
| Max (%) | 0.05 | 0.20 | 0.05 | 0.020 | |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties