Find suppliers for this alloy
C14420
| Elements | |||
|---|---|---|---|
| Cu(1,2) | Sn | Te | |
|
(1) Cu value includes Ag. (2) Includes Te + Sn. |
|||
| Min (%) | 99.90 | 0.04 | 0.005 |
| Max (%) | 0.15 | 0.05 | |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Automotive | Fins, Auto Radiator | Conductivity (Thermal) | Thermal Conductivity |
| Fins, Auto Radiator | Corrosion Resistance | Corrosion Resistance | |
| Fins, Auto Radiator | Mechanical Properties | Moderate Strength | |
| Fins, Auto Radiator | Softening Resistance | Resistance to Softening at Soldering Temperatures | |
| Fins, Auto Radiator | Welding Characteristics | Weldability | |
| Fins, Heat Exchanger | Conductivity (Thermal) | Thermal Conductivity | |
| Fins, Heat Exchanger | Corrosion Resistance | Corrosion Resistance | |
| Fins, Heat Exchanger | Mechanical Properties | Moderate Strength | |
| Fins, Heat Exchanger | Softening Resistance | Resistance to Softening at Soldering Temperatures | |
| Fins, Heat Exchanger | Welding Characteristics | Weldability |
| Form | Specific Sub-Form | Application | System | Standard | Description |
|---|---|---|---|---|---|
| Bar | ASTM | B152/B152M | COPPER SHEET, STRIP, PLATE AND ROLLED BAR | ||
| Plate | ASTM | B152/B152M | COPPER SHEET, STRIP, PLATE AND ROLLED BAR | ||
| Sheet | ASTM | B152/B152M | COPPER SHEET, STRIP, PLATE AND ROLLED BAR | ||
| Sheet, Strip, Roller Bar & Plate | ASME | SB152 | COPPER SHEET, STRIP, PLATE, AND ROLLED BAR | ||
| Strip | ASTM | B152/B152M | COPPER SHEET, STRIP, PLATE AND ROLLED BAR |
Corrosion Properties