Find suppliers for this alloyC14425
Chemical Composition
Element
Cu(1,2)PbSnZnFePNi(3)
(1) Cu + Sum of Named Elements, 99.97% Min. (2) Cu value includes Ag. (3) Includes Co.
Min (%)99.970.25
Max (%)0.100.350.100.0200.0100.020
Mechanical Properties*
Form
Temper
Temper Code
Tensile Strength
(ksi)
Elongation
(%)
Section Size
(in)
WireHard-drawn Electrical WireH86116   Typ
1   Typ
0.01
* Measured at room temperature, 68°F (20°C).
Physical Properties
Melting Point - Liquidus°F1967
Melting Point - Solidus°F1949
Densitylb/cu in. at 68°F0.321
Specific Gravity8.93
Electrical Conductivity% IACS at 68°F72
Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F169
Coefficient of Thermal Expansion 68-57210⁻⁶ per °F (68 – 572°F)10.1
Specific Heat CapacityBtu/ lb /°F at 68°F0.09
Modulus of Elasticity in Tensionksi18850
Poisson's Ratio0.34
Fabrication Properties
Technique Suitability
SolderingExcellent
BrazingExcellent
Oxyacetylene WeldingGood
Gas Shielded Arc WeldingExcellent
Coated Metal Arc WeldingNot Recommended
Spot WeldFair
Seam WeldNot Recommended
Butt WeldPoor
Machinability Rating20
Fabrication Process Properties

No fabrication process properties for this alloy

Thermal Characteristics

No thermal characteristics for this alloy

Typical uses
Product Category Product Reason Category Reason
ElectricalConductor Wire
Applicable Specifications

No applicable specifications for this alloy

Corrosion Properties