Find suppliers for this alloy
C14435
| Elements | |||
|---|---|---|---|
| Cu(1) | Sn | O | |
|
(1) Cu + Sum of Named Elements 99.7% min. |
|||
| Min (%) | 99.4 | 0.30 | |
| Max (%) | 0.60 | 0.001 | |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
Elongation (%) |
Vickers Hardness, 500 gm |
|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | |||||
| Strip | Annealed | O61 |
39.16 Typ |
50 Typ |
0.2 Typ |
| Tube | Annealed | O61 |
39.16 Min |
50 Typ |
0.2 Typ |
Physical Properties
| Technique | Suitability |
|---|---|
| Soldering | Excellent |
| Brazing | Excellent |
| Oxyacetylene Welding | Good |
| Gas Shielded Arc Welding | Good |
| Coated Metal Arc Welding | Good |
| Spot Weld | Good |
| Seam Weld | Good |
| Butt Weld | Good |
| Capacity for Being Cold Worked | Good |
| Capacity for Being Hot Formed | Good |
Common Fabrication Processes
Typical Uses
Applicable Specifications
Corrosion Properties