Find suppliers for this alloyC15150
Chemical Composition
Element
Cu(1)Zr
(1) Cu value includes Ag.
Min (%)99.900.015
Max (%)0.030
Mechanical Properties*
Form
Temper
Temper Code
Tensile Strength
(ksi)
Elongation
(%)
Flat ProductsHardH0453   Typ
3   Min
* Measured at room temperature, 68°F (20°C).
Physical Properties
Melting Point - Liquidus°F1976
Melting Point - Solidus°F1796
Densitylb/cu in. at 68°F0.322
Specific Gravity8.9
Electrical Conductivity% IACS at 68°F96
Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F215
Coefficient of Thermal Expansion 68-21210⁻⁶ per °F (68 – 212°F)10.2
Specific Heat CapacityBtu/ lb /°F at 68°F0.092
Modulus of Elasticity in Tensionksi17500
Modulus of Rigidityksi6500
Poisson's Ratio0.33
Fabrication Properties

No fabrication properties for this alloy

Fabrication Process Properties

No fabrication process properties for this alloy

    
Thermal Properties
Treatment Minimum* Maximum* Time**
* Temperature is measured in Fahrenheit. ** Time is measured in minutes.
Solution Treatment0
Annealing450500
Typical Uses

No information available.

Applicable Specifications

No applicable specifications for this alloy

Corrosion Properties

No information available.