Find suppliers for this alloyC15630
Chemical Composition
Element
Cu(1)PNi
(1) Cu + Sum of Named Elements 99.5% min.
Min (%)0.0150.60
Max (%)Rem0.0400.90
Mechanical Properties*
Form
Temper
Temper Code
Tensile Strength
(ksi)
YS-0.5% Ext
(ksi)
Elongation
(%)
Rockwell 15T
TubeAnnealedO6129.7   Min
8   Min
40   Min
55   Max
* Measured at room temperature, 68°F (20°C).
Physical Properties
Melting Point - Liquidus°F2156
Melting Point - Solidus°F1985
Densitylb/cu in. at 68°F0.323
Specific Gravity8.94
Coefficient of Thermal Expansion 68-57210⁻⁶ per °F (68 – 572°F)9.8
Modulus of Elasticity in Tensionksi17000
Modulus of Rigidityksi6400
Magnetic Permeability0.8
Poisson's Ratio0.35
Fabrication Properties
Technique Suitability
SolderingGood
BrazingGood
Oxyacetylene WeldingGood
Gas Shielded Arc WeldingGood
Coated Metal Arc WeldingGood
Spot WeldPoor
Seam WeldPoor
Butt WeldPoor
Capacity for Being Cold WorkedGood
Capacity for Being Hot FormedGood
Machinability Rating20
Fabrication Process Properties

No fabrication process properties for this alloy

Thermal Characteristics

No thermal characteristics for this alloy

Typical uses
Product Category Product Reason Category Reason
IndustrialSeamless, Internally Fined Heat Exchanger Tube
Applicable Specifications

No applicable specifications for this alloy

Corrosion Properties

No information available.