Chemical Composition
Element
Cu(1)PbFeAlO
(1) Cu value includes Ag.
Min (%)99.710.080.07
Max (%)0.010.010.120.15
Mechanical Properties*
Form
Temper
Temper Code
Tensile Strength
(ksi)
YS-0.2% Offset
Elongation
(%)
Section Size
(in)
Cold Work
(%)
Rod74   Typ
68   Typ
10   Typ
0.39282
50   Typ
48   Typ
18   Typ
0.87513
65   Typ
62   Typ
12   Typ
0.62556
77   Typ
70   Typ
10   Typ
0.2493
60   Typ
58   Typ
16   Typ
0.7539
47   Typ
39   Typ
20   Typ
0.94
Rod & WireAnnealedO6147   Typ
40   Typ
20   Typ
0.24
O6147   Typ
40   Typ
0.04
O6150   Typ
42   Typ
0.02
Wire99   Typ
94   Typ
0.0399.8
66   Typ
61   Typ
0.0365
69   Typ
65   Typ
0.0285
105   Typ
100   Typ
0.0299.9
94   Typ
90   Typ
0.0499.5
82   Typ
78   Typ
0.0898.5
* Measured at room temperature, 68°F (20°C).
Physical Properties

No physical properties for this alloy

Fabrication Properties

No fabrication properties for this alloy

Fabrication Process Properties

No fabrication process properties for this alloy

Thermal Characteristics

No thermal characteristics for this alloy

Typical uses
Product Category Product Reason Category Reason
ElectricalConnectorsConductivity (Electrical)Electrical Conductivity
ConnectorsConductivity (Thermal)Thermal Conductivity
ConnectorsCorrosion ResistanceCorrosion Resistance
ConnectorsMechanical PropertiesRetains Strength at High Temperatures
Insulated WireConductivity (Electrical)Electrical Conductivity
Insulated WireConductivity (Thermal)Thermal Conductivity
Insulated WireCorrosion ResistanceCorrosion Resistance
Insulated WireMechanical PropertiesRetains Strength at High Temperatures
Lead WireConductivity (Electrical)Electrical Conductivity
Lead WireConductivity (Thermal)Thermal Conductivity
Lead WireCorrosion ResistanceCorrosion Resistance
Lead WireMechanical PropertiesRetains Strength at High Temperatures
Springs, Light Duty Current CarryingConductivity (Electrical)Electrical Conductivity
Springs, Light Duty Current CarryingConductivity (Thermal)Thermal Conductivity
Springs, Light Duty Current CarryingCorrosion ResistanceCorrosion Resistance
Springs, Light Duty Current CarryingMechanical PropertiesHigh Modulus of Elasticity
Springs, Light Duty Current CarryingMechanical PropertiesRetains Strength at High Temperatures
Thermocouple WireConductivity (Electrical)Electrical Conductivity
Thermocouple WireConductivity (Thermal)Thermal Conductivity
Thermocouple WireCorrosion ResistanceCorrosion Resistance
Thermocouple WireMechanical PropertiesRetains Strength at High Temperatures
IndustrialHeat SinksConductivity (Electrical)Electrical Conductivity
Heat SinksConductivity (Thermal)Thermal Conductivity
Heat SinksCorrosion ResistanceCorrosion Resistance
Heat SinksMechanical PropertiesRetains Strength at High Temperatures
Resistance Welding ElectrodesConductivity (Electrical)Electrical Conductivity
Resistance Welding ElectrodesConductivity (Thermal)Thermal Conductivity
Resistance Welding ElectrodesCorrosion ResistanceOxidation Resistance
Resistance Welding ElectrodesSoftening ResistanceResistance to Thermal Softening
Applicable Specifications

No applicable specifications for this alloy

Corrosion Properties

No information available.