Find suppliers for this alloy
C15725
| Elements | |||||
|---|---|---|---|---|---|
| Cu(1) | Pb | Fe | Al(2) | O(3) | |
|
(1) Cu value includes Ag. (2) All aluminum present as Al2O3; 0.04% oxygen present as Cu2O with a negligible amount in solid solution with copper. (3) All aluminum present as Al2O3; 0.04% oxygen present as Cu2O with a negligible amount in solid solution with copper. |
|||||
| Min (%) | 99.43 | 0.23 | 0.20 | ||
| Max (%) | 0.01 | 0.01 | 0.27 | 0.28 | |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Electrical | Contactor Supports | Conductivity (Electrical) | Electrical Conductivity |
| Contactor Supports | Conductivity (Thermal) | Thermal Conductivity | |
| Contactor Supports | Corrosion Resistance | Corrosion Resistance | |
| Contactor Supports | Mechanical Properties | High Strength | |
| Contactor Supports | Mechanical Properties | Retains Strength at High Temperatures | |
| High Field Magnetic Coils | Conductivity (Electrical) | Electrical Conductivity | |
| High Field Magnetic Coils | Conductivity (Thermal) | Thermal Conductivity | |
| High Field Magnetic Coils | Corrosion Resistance | Corrosion Resistance | |
| High Field Magnetic Coils | Mechanical Properties | High Strength | |
| High Field Magnetic Coils | Mechanical Properties | Retains Strength at High Temperatures | |
| High Field Magnetic Coils | Solderability | Solderability | |
| High Speed Commutator | Conductivity (Electrical) | Electrical Conductivity | |
| High Speed Commutator | Conductivity (Thermal) | Thermal Conductivity | |
| High Speed Commutator | Corrosion Resistance | Corrosion Resistance | |
| High Speed Commutator | Mechanical Properties | High Strength | |
| Hybrid Circuit Packages | Conductivity (Electrical) | Electrical Conductivity | |
| Hybrid Circuit Packages | Conductivity (Thermal) | Thermal Conductivity | |
| Hybrid Circuit Packages | Corrosion Resistance | Corrosion Resistance | |
| Hybrid Circuit Packages | Mechanical Properties | High Strength | |
| Hybrid Circuit Packages | Mechanical Properties | Retains Strength at High Temperatures | |
| Hybrid Circuit Packages | Solderability | Solderability | |
| Incandescent Lamp Leads | Conductivity (Electrical) | Electrical Conductivity | |
| Incandescent Lamp Leads | Conductivity (Thermal) | Thermal Conductivity | |
| Incandescent Lamp Leads | Corrosion Resistance | Corrosion Resistance | |
| Incandescent Lamp Leads | Mechanical Properties | High Strength | |
| Incandescent Lamp Leads | Mechanical Properties | Retains Strength at High Temperatures | |
| Incandescent Lamp Leads | Solderability | Solderability | |
| Lead Frames | Conductivity (Electrical) | Electrical Conductivity | |
| Lead Frames | Conductivity (Thermal) | Thermal Conductivity | |
| Lead Frames | Corrosion Resistance | Corrosion Resistance | |
| Lead Frames | Finishing Characteristics | Photoetchability | |
| Lead Frames | Mechanical Properties | High Strength | |
| Lead Frames | Plating Characteristics | Plateable | |
| Microwave Power Tube Components | Conductivity (Electrical) | Electrical Conductivity | |
| Microwave Power Tube Components | Conductivity (Thermal) | Thermal Conductivity | |
| Microwave Power Tube Components | Corrosion Resistance | Corrosion Resistance | |
| Microwave Power Tube Components | Mechanical Properties | High Strength | |
| Microwave Power Tube Components | Mechanical Properties | Retains Strength at High Temperatures | |
| Microwave Power Tube Components | Solderability | Solderability | |
| Relay Blades for Electrical Switches | Conductivity (Electrical) | Electrical Conductivity | |
| Relay Blades for Electrical Switches | Conductivity (Thermal) | Thermal Conductivity | |
| Relay Blades for Electrical Switches | Mechanical Properties | Fatigue Life | |
| Relay Blades for Electrical Switches | Mechanical Properties | High Endurance Limit | |
| Relay Blades for Electrical Switches | Mechanical Properties | High Strength | |
| Relay Blades for Electrical Switches | Mechanical Properties | Maintains Strength after Exposure to Brazing Temp. | |
| X-ray Tube Components | Conductivity (Electrical) | Electrical Conductivity | |
| X-ray Tube Components | Conductivity (Thermal) | Thermal Conductivity | |
| X-ray Tube Components | Corrosion Resistance | Corrosion Resistance | |
| X-ray Tube Components | Mechanical Properties | High Strength | |
| X-ray Tube Components | Mechanical Properties | Retains Strength at High Temperatures | |
| X-ray Tube Components | Solderability | Solderability | |
| Industrial | Anode Stems for Chlorine Cells | Conductivity (Electrical) | Electrical Conductivity |
| Anode Stems for Chlorine Cells | Corrosion Resistance | Corrosion Resistance | |
| Anode Stems for Chlorine Cells | Mechanical Properties | Maintains Strength after Exposure to Brazing Temp. | |
| Conductors, Resistance Welding Equipment | Bearing Properties | Non-Stick to Coated Steels | |
| Conductors, Resistance Welding Equipment | Friction & Wear Properties | Wear Resistance | |
| Conductors, Resistance Welding Equipment | Mechanical Properties | High Strength | |
| Grounding Contacts for Arc Welders | Conductivity (Electrical) | Electrical Conductivity | |
| Grounding Contacts for Arc Welders | Conductivity (Thermal) | Thermal Conductivity | |
| Grounding Contacts for Arc Welders | Mechanical Properties | High Strength | |
| Spot Welding Electrodes | Bearing Properties | Non-Stick to Coated Steels | |
| Spot Welding Electrodes | Conductivity (Electrical) | Electrical Conductivity | |
| Spot Welding Electrodes | Conductivity (Thermal) | Thermal Conductivity | |
| Spot Welding Electrodes | Friction & Wear Properties | Wear Resistance | |
| Spot Welding Electrodes | Mechanical Properties | High Strength | |
| Welding Back-up Bars | Bearing Properties | Non-Stick to Coated Steels | |
| Welding Back-up Bars | Friction & Wear Properties | Wear Resistance | |
| Welding Back-up Bars | Mechanical Properties | High Strength | |
| Welding Back-up Bars | Mechanical Properties | Retains Strength at High Temperatures |
Applicable Specifications
Corrosion Properties