Find suppliers for this alloyC15725
Chemical Composition
Element
Cu(1)PbFeAl(2)O(3)
(1) Cu value includes Ag. (2) All aluminum present as Al2O3; 0.04% oxygen present as Cu2O with a negligible amount in solid solution with copper. (3) All aluminum present as Al2O3; 0.04% oxygen present as Cu2O with a negligible amount in solid solution with copper.
Min (%)99.430.230.20
Max (%)0.010.010.270.28
Mechanical Properties

No mechanical properties for this alloy

Physical Properties

No physical properties for this alloy

Fabrication Properties

No fabrication properties for this alloy

Fabrication Process Properties

No fabrication process properties for this alloy

Thermal Characteristics

No thermal characteristics for this alloy

Typical uses
Product Category Product Reason Category Reason
ElectricalContactor SupportsConductivity (Electrical)Electrical Conductivity
Contactor SupportsConductivity (Thermal)Thermal Conductivity
Contactor SupportsCorrosion ResistanceCorrosion Resistance
Contactor SupportsMechanical PropertiesHigh Strength
Contactor SupportsMechanical PropertiesRetains Strength at High Temperatures
High Field Magnetic CoilsConductivity (Electrical)Electrical Conductivity
High Field Magnetic CoilsConductivity (Thermal)Thermal Conductivity
High Field Magnetic CoilsCorrosion ResistanceCorrosion Resistance
High Field Magnetic CoilsMechanical PropertiesHigh Strength
High Field Magnetic CoilsMechanical PropertiesRetains Strength at High Temperatures
High Field Magnetic CoilsSolderabilitySolderability
High Speed CommutatorConductivity (Electrical)Electrical Conductivity
High Speed CommutatorConductivity (Thermal)Thermal Conductivity
High Speed CommutatorCorrosion ResistanceCorrosion Resistance
High Speed CommutatorMechanical PropertiesHigh Strength
Hybrid Circuit PackagesConductivity (Electrical)Electrical Conductivity
Hybrid Circuit PackagesConductivity (Thermal)Thermal Conductivity
Hybrid Circuit PackagesCorrosion ResistanceCorrosion Resistance
Hybrid Circuit PackagesMechanical PropertiesHigh Strength
Hybrid Circuit PackagesMechanical PropertiesRetains Strength at High Temperatures
Hybrid Circuit PackagesSolderabilitySolderability
Incandescent Lamp LeadsConductivity (Electrical)Electrical Conductivity
Incandescent Lamp LeadsConductivity (Thermal)Thermal Conductivity
Incandescent Lamp LeadsCorrosion ResistanceCorrosion Resistance
Incandescent Lamp LeadsMechanical PropertiesHigh Strength
Incandescent Lamp LeadsMechanical PropertiesRetains Strength at High Temperatures
Incandescent Lamp LeadsSolderabilitySolderability
Lead FramesConductivity (Electrical)Electrical Conductivity
Lead FramesConductivity (Thermal)Thermal Conductivity
Lead FramesCorrosion ResistanceCorrosion Resistance
Lead FramesFinishing CharacteristicsPhotoetchability
Lead FramesMechanical PropertiesHigh Strength
Lead FramesPlating CharacteristicsPlateable
Microwave Power Tube ComponentsConductivity (Electrical)Electrical Conductivity
Microwave Power Tube ComponentsConductivity (Thermal)Thermal Conductivity
Microwave Power Tube ComponentsCorrosion ResistanceCorrosion Resistance
Microwave Power Tube ComponentsMechanical PropertiesHigh Strength
Microwave Power Tube ComponentsMechanical PropertiesRetains Strength at High Temperatures
Microwave Power Tube ComponentsSolderabilitySolderability
Relay Blades for Electrical SwitchesConductivity (Electrical)Electrical Conductivity
Relay Blades for Electrical SwitchesConductivity (Thermal)Thermal Conductivity
Relay Blades for Electrical SwitchesMechanical PropertiesFatigue Life
Relay Blades for Electrical SwitchesMechanical PropertiesHigh Endurance Limit
Relay Blades for Electrical SwitchesMechanical PropertiesHigh Strength
Relay Blades for Electrical SwitchesMechanical PropertiesMaintains Strength after Exposure to Brazing Temp.
X-ray Tube ComponentsConductivity (Electrical)Electrical Conductivity
X-ray Tube ComponentsConductivity (Thermal)Thermal Conductivity
X-ray Tube ComponentsCorrosion ResistanceCorrosion Resistance
X-ray Tube ComponentsMechanical PropertiesHigh Strength
X-ray Tube ComponentsMechanical PropertiesRetains Strength at High Temperatures
X-ray Tube ComponentsSolderabilitySolderability
IndustrialAnode Stems for Chlorine CellsConductivity (Electrical)Electrical Conductivity
Anode Stems for Chlorine CellsCorrosion ResistanceCorrosion Resistance
Anode Stems for Chlorine CellsMechanical PropertiesMaintains Strength after Exposure to Brazing Temp.
Conductors, Resistance Welding EquipmentBearing PropertiesNon-Stick to Coated Steels
Conductors, Resistance Welding EquipmentFriction & Wear PropertiesWear Resistance
Conductors, Resistance Welding EquipmentMechanical PropertiesHigh Strength
Grounding Contacts for Arc WeldersConductivity (Electrical)Electrical Conductivity
Grounding Contacts for Arc WeldersConductivity (Thermal)Thermal Conductivity
Grounding Contacts for Arc WeldersMechanical PropertiesHigh Strength
Spot Welding ElectrodesBearing PropertiesNon-Stick to Coated Steels
Spot Welding ElectrodesConductivity (Electrical)Electrical Conductivity
Spot Welding ElectrodesConductivity (Thermal)Thermal Conductivity
Spot Welding ElectrodesFriction & Wear PropertiesWear Resistance
Spot Welding ElectrodesMechanical PropertiesHigh Strength
Welding Back-up BarsBearing PropertiesNon-Stick to Coated Steels
Welding Back-up BarsFriction & Wear PropertiesWear Resistance
Welding Back-up BarsMechanical PropertiesHigh Strength
Welding Back-up BarsMechanical PropertiesRetains Strength at High Temperatures
Applicable Specifications

No applicable specifications for this alloy

Corrosion Properties

No information available.