Find suppliers for this alloy
C15735
| Elements | |||||
|---|---|---|---|---|---|
| Cu(1) | Pb | Fe | Al | O | |
|
(1) Cu value includes Ag. |
|||||
| Min (%) | 99.24 | 0.33 | 0.29 | ||
| Max (%) | 0.01 | 0.01 | 0.37 | 0.37 | |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.2% Offset (ksi) |
Elongation (%) |
Section Size (in) |
|---|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | ||||||
| Rod | As Hot Extruded | M30 |
82 Typ |
78 Typ |
13 Typ |
3 |
| As Hot Extruded | M30 |
71 Typ |
60 Typ |
16 Typ |
2.5 | |
| As Hot Extruded | M30 |
75 Typ |
70 Typ |
13 Typ |
4.7 | |
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Electrical | Circuit Breakers | Conductivity (Electrical) | Electrical Conductivity |
| Circuit Breakers | Conductivity (Thermal) | Thermal Conductivity | |
| Circuit Breakers | Corrosion Resistance | Corrosion Resistance | |
| Circuit Breakers | Mechanical Properties | High Strength | |
| Circuit Breakers | Mechanical Properties | Retains Strength at High Temperatures | |
| Conductors | Conductivity (Electrical) | Electrical Conductivity | |
| Conductors | Conductivity (Thermal) | Thermal Conductivity | |
| Conductors | Corrosion Resistance | Corrosion Resistance | |
| Conductors | Mechanical Properties | High Strength | |
| Conductors | Mechanical Properties | Retains Strength at High Temperatures | |
| Heat Sinks, Feed Through Type | Conductivity (Electrical) | Electrical Conductivity | |
| Heat Sinks, Feed Through Type | Conductivity (Thermal) | Thermal Conductivity | |
| Heat Sinks, Feed Through Type | Corrosion Resistance | Corrosion Resistance | |
| Heat Sinks, Feed Through Type | Mechanical Properties | High Strength | |
| Heat Sinks, Feed Through Type | Mechanical Properties | Retains Strength at High Temperatures | |
| Motor Parts | Conductivity (Electrical) | Electrical Conductivity | |
| Motor Parts | Conductivity (Thermal) | Thermal Conductivity | |
| Motor Parts | Corrosion Resistance | Corrosion Resistance | |
| Motor Parts | Mechanical Properties | High Strength | |
| Motor Parts | Mechanical Properties | Retains Strength at High Temperatures | |
| Industrial | Resistance Welding Electrodes | Conductivity (Electrical) | Electrical Conductivity |
| Resistance Welding Electrodes | Conductivity (Thermal) | Thermal Conductivity | |
| Resistance Welding Electrodes | Corrosion Resistance | Oxidation Resistance | |
| Resistance Welding Electrodes | Softening Resistance | Resistance to Thermal Softening |
Applicable Specifications