Find suppliers for this alloyC15735
Element | |||||
---|---|---|---|---|---|
Cu(1) | Pb | Fe | Al | O | |
(1) Cu value includes Ag. | |||||
Min (%) | 99.24 | 0.33 | 0.29 | ||
Max (%) | 0.01 | 0.01 | 0.37 | 0.37 |
Form | Temper | Temper Code | Tensile Strength (ksi) | YS-0.2% Offset | Elongation (%) | Section Size (in) | |
---|---|---|---|---|---|---|---|
Rod | As Hot Extruded | M30 | 82 Typ | 78 Typ | 13 Typ | 3 | |
M30 | 71 Typ | 60 Typ | 16 Typ | 2.5 | |||
M30 | 75 Typ | 70 Typ | 13 Typ | 4.7 | |||
* Measured at room temperature, 68°F (20°C). |
Physical Properties
Fabrication Properties
Fabrication Process Properties
Thermal Characteristics
Product Category | Product | Reason Category | Reason |
---|---|---|---|
Electrical | Circuit Breakers | Conductivity (Electrical) | Electrical Conductivity |
Circuit Breakers | Conductivity (Thermal) | Thermal Conductivity | |
Circuit Breakers | Corrosion Resistance | Corrosion Resistance | |
Circuit Breakers | Mechanical Properties | High Strength | |
Circuit Breakers | Mechanical Properties | Retains Strength at High Temperatures | |
Conductors | Conductivity (Electrical) | Electrical Conductivity | |
Conductors | Conductivity (Thermal) | Thermal Conductivity | |
Conductors | Corrosion Resistance | Corrosion Resistance | |
Conductors | Mechanical Properties | High Strength | |
Conductors | Mechanical Properties | Retains Strength at High Temperatures | |
Heat Sinks, Feed Through Type | Conductivity (Electrical) | Electrical Conductivity | |
Heat Sinks, Feed Through Type | Conductivity (Thermal) | Thermal Conductivity | |
Heat Sinks, Feed Through Type | Corrosion Resistance | Corrosion Resistance | |
Heat Sinks, Feed Through Type | Mechanical Properties | High Strength | |
Heat Sinks, Feed Through Type | Mechanical Properties | Retains Strength at High Temperatures | |
Motor Parts | Conductivity (Electrical) | Electrical Conductivity | |
Motor Parts | Conductivity (Thermal) | Thermal Conductivity | |
Motor Parts | Corrosion Resistance | Corrosion Resistance | |
Motor Parts | Mechanical Properties | High Strength | |
Motor Parts | Mechanical Properties | Retains Strength at High Temperatures | |
Industrial | Resistance Welding Electrodes | Conductivity (Electrical) | Electrical Conductivity |
Resistance Welding Electrodes | Conductivity (Thermal) | Thermal Conductivity | |
Resistance Welding Electrodes | Corrosion Resistance | Oxidation Resistance | |
Resistance Welding Electrodes | Softening Resistance | Resistance to Thermal Softening |