Find suppliers for this alloy
C15750
| Elements | |||||
|---|---|---|---|---|---|
| Cu(1) | Fe | Al(2) | B | O(3) | |
|
(1) Cu value includes Ag. (2) All aluminum present as Al2O3; 0.04% oxygen present as Cu2O with a negligible amount in solid solution with copper. (3) All aluminum present as Al2O3; 0.04% oxygen present as Cu2O with a negligible amount in solid solution with copper. |
|||||
| Min (%) | 98.56 | 0.42 | 0.52 | ||
| Max (%) | 0.04 | 0.50 | 0.22 | 0.68 | |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.5% Ext (ksi) |
Elongation (%) |
Rockwell B scale |
|---|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | ||||||
| Rod & Bar | As Hot Extruded | M30 |
65 Min 70 Typ 75 Max |
52 Min 55 Typ |
15 Min 20 Max |
75 Min 80 Max |
| Melting Point - Liquidus°F | 1981 |
|---|---|
| Densitylb/cu in. at 68°F | 0.312 |
| Specific Gravity | 8.65 |
| Technique | Suitability |
|---|---|
| Soldering | Good |
| Brazing | Good |
| Oxyacetylene Welding | Not Recommended |
| Coated Metal Arc Welding | Not Recommended |
| Spot Weld | Poor |
| Seam Weld | Poor |
| Butt Weld | Poor |
| Capacity for Being Cold Worked | Excellent |
| Capacity for Being Hot Formed | Poor |
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties