Find suppliers for this alloyC15760
Chemical Composition
Element
Cu(1)PbFeAl(2)O(3)
(1) Cu value includes Ag. (2) All aluminum present as Al2O3; 0.04% oxygen present as Cu2O with a negligible amount in solid solution with copper. (3) All aluminum present as Al2O3; 0.04% oxygen present as Cu2O with a negligible amount in solid solution with copper.
Min (%)98.770.580.52
Max (%)0.010.010.620.59
Mechanical Properties*
Form
Temper
Temper Code
Tensile Strength
(ksi)
YS-0.2% Offset
Elongation
(%)
Rockwell B scale
Fatigue Strength**
(ksi)
Section Size
(in)
Cold Work
(%)
BarAs Hot ExtrudedM3070   Typ
65   Typ
17   Typ
78   Typ
0.5
RodAnnealedO6176   Typ
71   Typ
18   Typ
77   Typ
0.275
O6189   Typ
85   Typ
16   Typ
84   Typ
0.275
O6184   Typ
79   Typ
18   Typ
80   Typ
0.275
As Hot ExtrudedM3072   Typ
69   Typ
14   Typ
80   Typ
2.5
M3080   Typ
75   Typ
22   Typ
80   Typ
0.54
HardH0490   Typ
87   Typ
14   Typ
86   Typ
36   Typ
0.27574
H0483   Typ
79   Typ
16   Typ
83   Typ
0.514
* Measured at room temperature, 68°F (20°C). ** Fatigue Strength: 100 x 106 cycles, unless indicated as [N] x 106.
Physical Properties
Melting Point - Liquidus°F1981
Melting Point - Solidus°F1981
Densitylb/cu in. at 68°F0.318
Specific Gravity8.81
Electrical Conductivity% IACS at 68°F78
Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F186
Coefficient of Thermal Expansion 68-57210⁻⁶ per °F (68 – 572°F)9.2
Specific Heat CapacityBtu/ lb /°F at 68°F0.09
Modulus of Elasticity in Tensionksi17000
Fabrication Properties
Technique Suitability Footnote
SolderingExcellent
BrazingGood
Oxyacetylene WeldingNot Recommended
Gas Shielded Arc WeldingNot Recommended
Coated Metal Arc WeldingNot Recommended
Spot WeldPoor
Seam WeldPoor
Butt WeldFair
Capacity for Being Cold WorkedExcellent
Capacity for Being Hot FormedPoorPoor in wrought form.
Common Fabrication Processes
  • Blanking
  • Cold working
  • Drawing
  • Extruding
  • Forging
  • heading
  • Hot isostatic pressing of powder
  • Hot working
  • Machining
  • Roll Threading and Knurling
  • Rolling
  • Swaging
  • Upsetting
    
Thermal Properties
Treatment Minimum* Maximum*
* Temperature is measured in Fahrenheit.
Annealing12001800
Typical uses
Product Category Product Reason Category Reason
ElectricalContactor SupportsConductivity (Electrical)Electrical Conductivity
Contactor SupportsConductivity (Thermal)Thermal Conductivity
Contactor SupportsCorrosion ResistanceCorrosion Resistance
Contactor SupportsMechanical PropertiesHigh Strength
Contactor SupportsMechanical PropertiesRetains Strength at High Temperatures
Contactor SupportsSolderabilitySolderability
Electronic Lead FramesConductivity (Electrical)Electrical Conductivity
Electronic Lead FramesConductivity (Thermal)Thermal Conductivity
Electronic Lead FramesCorrosion ResistanceCorrosion Resistance
Electronic Lead FramesMechanical PropertiesHigh Strength
Electronic Lead FramesMechanical PropertiesRetains Strength at High Temperatures
Electronic Lead FramesSolderabilitySolderability
High-Field Magnetic CoilsConductivity (Electrical)Electrical Conductivity
High-Field Magnetic CoilsConductivity (Thermal)Thermal Conductivity
High-Field Magnetic CoilsCorrosion ResistanceCorrosion Resistance
High-Field Magnetic CoilsMechanical PropertiesHigh Strength
High-Field Magnetic CoilsMechanical PropertiesRetains Strength at High Temperatures
High-Field Magnetic CoilsSolderabilitySolderability
Hybrid Circuit PackagesConductivity (Electrical)Electrical Conductivity
Hybrid Circuit PackagesConductivity (Thermal)Thermal Conductivity
Hybrid Circuit PackagesCorrosion ResistanceCorrosion Resistance
Hybrid Circuit PackagesMechanical PropertiesHigh Strength
Hybrid Circuit PackagesMechanical PropertiesRetains Strength at High Temperatures
Hybrid Circuit PackagesSolderabilitySolderability
Incandescent Lamp LeadsConductivity (Electrical)Electrical Conductivity
Incandescent Lamp LeadsConductivity (Thermal)Thermal Conductivity
Incandescent Lamp LeadsCorrosion ResistanceCorrosion Resistance
Incandescent Lamp LeadsMechanical PropertiesHigh Strength
Incandescent Lamp LeadsMechanical PropertiesRetains Strength at High Temperatures
Incandescent Lamp LeadsSolderabilitySolderability
Microwave Power Tube ComponentsConductivity (Electrical)Electrical Conductivity
Microwave Power Tube ComponentsConductivity (Thermal)Thermal Conductivity
Microwave Power Tube ComponentsCorrosion ResistanceCorrosion Resistance
Microwave Power Tube ComponentsMechanical PropertiesHigh Strength
Microwave Power Tube ComponentsMechanical PropertiesRetains Strength at High Temperatures
Microwave Power Tube ComponentsSolderabilitySolderability
Relay BladesConductivity (Electrical)Electrical Conductivity
Relay BladesConductivity (Thermal)Thermal Conductivity
Relay BladesCorrosion ResistanceCorrosion Resistance
Relay BladesMechanical PropertiesHigh Strength
Relay BladesMechanical PropertiesRetains Strength at High Temperatures
Relay BladesSolderabilitySolderability
X-ray Tube ComponentsConductivity (Electrical)Electrical Conductivity
X-ray Tube ComponentsConductivity (Thermal)Thermal Conductivity
X-ray Tube ComponentsCorrosion ResistanceCorrosion Resistance
X-ray Tube ComponentsMechanical PropertiesHigh Strength
X-ray Tube ComponentsMechanical PropertiesRetains Strength at High Temperatures
X-ray Tube ComponentsSolderabilitySolderability
IndustrialBack-up bars for WeldingBearing PropertiesNon-Stick to Coated Steels
Back-up bars for WeldingConductivity (Thermal)Thermal Conductivity
High Flux ElectromagnetsConductivity (Electrical)Electrical Conductivity
High Flux ElectromagnetsConductivity (Thermal)Thermal Conductivity
High Flux ElectromagnetsMechanical PropertiesHigh Strength
Mig Welding TipsBearing PropertiesNon-Sticking of Weld Splatter
Mig Welding TipsFriction & Wear PropertiesLow Wear Rate of Feed Hole
Mig Welding TipsMachining CharacteristicsDowntime for Cleaning and Change-Over Reduced
Mig Welding TipsMechanical PropertiesHigh Strength
Molds for Continuous Casting MachinesConductivity (Thermal)Thermal Conductivity
Molds for Continuous Casting MachinesCorrosion ResistanceCorrosion Resistance
Molds for Continuous Casting MachinesMechanical PropertiesHigh Strength
Molds for Continuous Casting MachinesMechanical PropertiesRetains Strength at High Temperatures
Resistance Welding ElectrodesConductivity (Electrical)Electrical Conductivity
Resistance Welding ElectrodesConductivity (Thermal)Thermal Conductivity
Resistance Welding ElectrodesCorrosion ResistanceCorrosion Resistance
Resistance Welding ElectrodesMechanical PropertiesRetains Strength at High Temperatures
Resistance Welding ElectrodesSoftening ResistanceResistance to Thermal Softening
Seam Welding WheelsConductivity (Electrical)Electrical Conductivity
Seam Welding WheelsConductivity (Thermal)Thermal Conductivity
Seam Welding WheelsCorrosion ResistanceCorrosion Resistance
Seam Welding WheelsMechanical PropertiesHigh Strength
Seam Welding WheelsMechanical PropertiesRetains Strength at High Temperatures
Side Dam Blocks for Hazelett Casting MachinesConductivity (Thermal)Thermal Conductivity
Side Dam Blocks for Hazelett Casting MachinesCorrosion ResistanceCorrosion Resistance
Side Dam Blocks for Hazelett Casting MachinesMechanical PropertiesHigh Strength
Side Dam Blocks for Hazelett Casting MachinesMechanical PropertiesRetains Strength at High Temperatures
Soldering Gun TipsConductivity (Thermal)Thermal Conductivity
Soldering Gun TipsCorrosion ResistanceCorrosion Resistance
Soldering Gun TipsMechanical PropertiesHigh Strength
Soldering Gun TipsMechanical PropertiesRetains Strength at High Temperatures
Spot Welding ElectrodesBearing PropertiesNon-Stick to Coated Steels
Spot Welding ElectrodesConductivity (Electrical)Electrical Conductivity
Spot Welding ElectrodesConductivity (Thermal)Thermal Conductivity
Applicable Specifications

No applicable specifications for this alloy

Corrosion Properties

No information available.