C15815
| Elements | ||||||
|---|---|---|---|---|---|---|
| Cu(1) | Pb | Fe | Al(2) | B | O(3) | |
|
(1) Cu value includes Ag. (2) All aluminum present as Al2O3; 0.04% oxygen present as Cu2O with a negligible amount in solid solution with copper. (3) All aluminum present as Al2O3; 0.04% oxygen present as Cu2O with a negligible amount in solid solution with copper. |
||||||
| Min (%) | 97.82 | 0.13 | 1.2 | |||
| Max (%) | 0.01 | 0.01 | 0.17 | 1.8 | 0.19 | |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
| Form | Specific Sub-Form | Application | System | Standard | Description |
|---|---|---|---|---|---|
| Bar | ASTM | B876 | BORATED DISPERSION STRENGTHENED COPPER PLATE, SHEET, STRIP AND ROLLED BAR FOR NUCLEAR APPLICATIONS | ||
| Plate | ASTM | B876 | BORATED DISPERSION STRENGTHENED COPPER PLATE, SHEET, STRIP AND ROLLED BAR FOR NUCLEAR APPLICATIONS | ||
| Sheet | ASTM | B876 | BORATED DISPERSION STRENGTHENED COPPER PLATE, SHEET, STRIP AND ROLLED BAR FOR NUCLEAR APPLICATIONS | ||
| Strip | ASTM | B876 | BORATED DISPERSION STRENGTHENED COPPER PLATE, SHEET, STRIP AND ROLLED BAR FOR NUCLEAR APPLICATIONS |
Corrosion Properties