Find suppliers for this alloy
C16400
| Elements | ||||
|---|---|---|---|---|
| Cu(1) | Sn | Fe | Cd | |
|
(1) Cu value includes Ag. |
||||
| Min (%) | 99.8 | 0.20 | 0.6 | |
| Max (%) | 0.40 | 0.02 | 0.9 | |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties