| Elements | ||||||||
|---|---|---|---|---|---|---|---|---|
| Cu(2,3) | Pb | Al | Be | Bi | Co(1) | Sb | Si | |
|
(1) Ni + Co 0.20% min.: Ni + Fe + Co 0.6% max. (2) Cu + Sum of Named Elements 99.5% min. (3) Cu value includes Ag. |
||||||||
| Min (%) | 1.80 | 0.005 | 0.20 | 0.005 | ||||
| Max (%) | Rem | 0.095 | 0.20 | 2.00 | 00.10 | 0.10 | 0.20 | |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.2% Offset (ksi) |
Elongation (%) |
Rockwell C scale |
|---|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | ||||||
| Rod | Hard and Precipitation Heat Treateed (HT) | TH04 |
185 Min 205 Typ 225 Max |
160 Min |
2 Typ |
39 Typ |
| Wire | Hard and Precipitation Heat Treateed (HT) | TH04 |
195 Min 212 Typ 230 Max |
40 Max | ||
| Melting Point - Liquidus°F | 1800 |
|---|---|
| Melting Point - Solidus°F | 1590 |
| Densitylb/cu in. at 68°F | 0.29 |
| Specific Gravity | 8.26 |
| Electrical Conductivity% IACS at 68°F | 22 |
| Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F | 62 |
| Coefficient of Thermal Expansion 68-57210 to -6 power per °F (68 – 572°F) | 9.9 |
| Modulus of Elasticity in Tensionksi | 18500 |
| Modulus of Rigidityksi | 7300 |
| Poisson's Ratioksi | 0.3 |
| Technique | Suitability |
|---|---|
| Soldering | Good |
| Brazing | Good |
| Oxyacetylene Welding | Not Recommended |
| Gas Shielded Arc Welding | Good |
| Coated Metal Arc Welding | Good |
| Capacity for Being Hot Formed | Excellent |
| Machinability Rating | 40 |
Common Fabrication Processes
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Electrical | Conductors, Electrical and Thermal, High Strength | ||
| Fasteners | Mechanical Properties |
| Form | Specific Sub-Form | Application | System | Standard | Description |
|---|---|---|---|---|---|
| Rod | B196/B196M | ASTM | COPPER BERYLLIUM ALLOY ROD AND BAR | ||
| Wire | B197/B197M | ASTM | COPPER BERYLLIUM ALLOY WIRE | ||
| 4725 | AMS | COPPER-BERYLLIUM ALLOY WIRE - SOLUTION HEAT TREATED |
Corrosion Properties