Find suppliers for this alloy
C17410
| Elements | ||||||
|---|---|---|---|---|---|---|
| Cu(1,2) | Fe | Al | Be | Co | Si | |
|
(1) Cu + Sum of Named Elements 99.5% min. (2) Cu value includes Ag. |
||||||
| Min (%) | 0.15 | 0.35 | ||||
| Max (%) | Rem | 0.20 | 0.20 | 0.50 | 0.6 | 0.20 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.2% Offset (ksi) |
Elongation (%) |
Rockwell B scale |
|---|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | ||||||
| Flat Products | 1/2 Hard and Precipitation Heat Treated | TH02 |
105 Typ |
90 Typ |
15 Typ |
93 Typ |
| Hard and Precipitation Heat Treated | TH04 |
120 Typ |
110 Typ |
12 Typ |
102 Typ |
|
| (1)Cold worked and aged. Actual value is 120-150. | |
| Melting Point - Liquidus°F | 1950 |
|---|---|
| Melting Point - Solidus°F | 1875 |
| Densitylb/cu in. at 68°F | 0.318 |
| Specific Gravity | 8.81 |
| Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F | 120 (1) |
| Modulus of Elasticity in Tensionksi | 19000 |
| Technique | Suitability |
|---|---|
| Soldering | Good |
| Brazing | Good |
| Oxyacetylene Welding | Not Recommended |
| Gas Shielded Arc Welding | Fair |
| Coated Metal Arc Welding | Fair |
| Spot Weld | Good |
| Seam Weld | Fair |
| Butt Weld | Fair |
| Capacity for Being Cold Worked | Excellent |
| Capacity for Being Hot Formed | Excellent |
Common Fabrication Processes
- Blanking
- Drilling
- Forming and Bending
- Tapping
- Turning
| Treatment | Minimum* | Maximum* | Time** | |
|---|---|---|---|---|
| * Temperature is measured in Fahrenheit. ** Time is measured in minutes. | ||||
| Hot Working Temperature | 1200 | 1750 | ||
| Solution Treatment | 0 | |||
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Electrical | Connectors | Conductivity (Electrical) | Electrical Conductivity |
| Connectors | Corrosion Resistance | Corrosion Resistance | |
| Connectors | Creep Properties | Creep Resistant | |
| Connectors | Mechanical Properties | High Strength | |
| Connectors | Mechanical Properties | Retains Strength at High Temperatures | |
| Connectors | Softening Resistance | Resistance to Thermal Softening | |
| Connectors | Solderability | Solderability | |
| Contacts | Conductivity (Electrical) | Electrical Conductivity | |
| Contacts | Corrosion Resistance | Corrosion Resistance | |
| Contacts | Creep Properties | Creep Resistant | |
| Contacts | Friction & Wear Properties | Wear Resistance | |
| Contacts | Mechanical Properties | High Strength | |
| Contacts | Softening Resistance | Resistance to Thermal Softening | |
| Contacts | Solderability | Solderability | |
| Current and Signal Carrying Springs | Conductivity (Electrical) | Electrical Conductivity | |
| Current and Signal Carrying Springs | Corrosion Resistance | Corrosion Resistance | |
| Current and Signal Carrying Springs | Creep Properties | Creep Resistant | |
| Current and Signal Carrying Springs | Mechanical Properties | Fatigue Resistance | |
| Current and Signal Carrying Springs | Mechanical Properties | High Strength | |
| Current and Signal Carrying Springs | Mechanical Properties | Retains Strength at High Temperatures | |
| Current and Signal Carrying Springs | Softening Resistance | Resistance to Thermal Softening | |
| Current and Signal Carrying Springs | Solderability | Solderability | |
| Electrical Switch and Relay Blades | Conductivity (Electrical) | Electrical Conductivity | |
| Electrical Switch and Relay Blades | Conductivity (Thermal) | Thermal Conductivity | |
| Electrical Switch and Relay Blades | Corrosion Resistance | Corrosion Resistance | |
| Electrical Switch and Relay Blades | Forming Characteristics | Formability, Good | |
| Electrical Switch and Relay Blades | Heat Treatability | Heat Treatable | |
| Electrical Switch and Relay Blades | Mechanical Properties | Fatigue Resistance | |
| Electrical Switch and Relay Blades | Mechanical Properties | High Endurance Limit | |
| Electrical Switch and Relay Blades | Mechanical Properties | High Strength | |
| Electrical Switch and Relay Blades | Thermal Properties | Resistance to Stress Relaxation | |
| Fuse Clips | Conductivity (Electrical) | Electrical Conductivity | |
| Fuse Clips | Corrosion Resistance | Corrosion Resistance | |
| Fuse Clips | Mechanical Properties | High Strength | |
| Fuse Clips | Solderability | Solderability | |
| Lead Frames | Conductivity (Electrical) | Electrical Conductivity | |
| Lead Frames | Corrosion Resistance | Corrosion Resistance | |
| Lead Frames | Creep Properties | Creep Resistant | |
| Lead Frames | Mechanical Properties | High Strength | |
| Lead Frames | Mechanical Properties | Retains Strength at High Temperatures | |
| Lead Frames | Softening Resistance | Resistance to Thermal Softening | |
| Lead Frames | Solderability | Solderability | |
| Switch Parts | Conductivity (Electrical) | Electrical Conductivity | |
| Switch Parts | Corrosion Resistance | Corrosion Resistance | |
| Switch Parts | Creep Properties | Creep Resistant | |
| Switch Parts | Mechanical Properties | High Strength | |
| Switch Parts | Softening Resistance | Resistance to Thermal Softening | |
| Terminals | Conductivity (Electrical) | Electrical Conductivity | |
| Terminals | Corrosion Resistance | Corrosion Resistance | |
| Terminals | Mechanical Properties | High Strength | |
| Terminals | Softening Resistance | Resistance to Thermal Softening | |
| Terminals | Solderability | Solderability | |
| Fasteners | Fasteners | Corrosion Resistance | Corrosion Resistance |
| Fasteners | Mechanical Properties | Very High Strength | |
| Industrial | Bellows | Corrosion Resistance | Corrosion Resistance |
| Bellows | Forming Characteristics | Formability | |
| Bellows | Mechanical Properties | Ductility | |
| Bellows | Mechanical Properties | Fatigue Resistance | |
| Bellows | Mechanical Properties | High Strength | |
| Diaphragms | Corrosion Resistance | Corrosion Resistance | |
| Diaphragms | Forming Characteristics | Formability | |
| Diaphragms | Mechanical Properties | Fatigue Resistance | |
| Diaphragms | Mechanical Properties | High Strength | |
| Die casting plunger tips | Conductivity (Electrical) | Electrical Conductivity | |
| Die casting plunger tips | Corrosion Resistance | Corrosion Resistance | |
| Die casting plunger tips | Creep Properties | Creep Resistant | |
| Die casting plunger tips | Friction & Wear Properties | Wear Resistance | |
| Die casting plunger tips | Mechanical Properties | High Strength | |
| Die casting plunger tips | Softening Resistance | Resistance to Thermal Softening | |
| Mechanical Springs | Corrosion Resistance | Corrosion Resistance | |
| Mechanical Springs | Mechanical Properties | Fatigue Resistance | |
| Mechanical Springs | Mechanical Properties | High Strength | |
| Mechanical Springs | Softening Resistance | Resistance to Thermal Softening | |
| Resistance and Spot Welding Tips | Conductivity (Electrical) | Electrical Conductivity | |
| Resistance and Spot Welding Tips | Corrosion Resistance | Corrosion Resistance | |
| Resistance and Spot Welding Tips | Mechanical Properties | High Strength | |
| Resistance Welding Electrodes | Conductivity (Electrical) | Electrical Conductivity | |
| Resistance Welding Electrodes | Conductivity (Thermal) | Thermal Conductivity | |
| Resistance Welding Electrodes | Corrosion Resistance | Oxidation Resistance | |
| Resistance Welding Electrodes | Softening Resistance | Resistance to Thermal Softening | |
| Sleeve Bearings | Conductivity (Electrical) | Electrical Conductivity | |
| Sleeve Bearings | Corrosion Resistance | Corrosion Resistance | |
| Sleeve Bearings | Creep Properties | Creep Resistant | |
| Sleeve Bearings | Friction & Wear Properties | Wear Resistance | |
| Sleeve Bearings | Mechanical Properties | High Strength | |
| Springs | Corrosion Resistance | Corrosion Resistance | |
| Springs | Mechanical Properties | Fatigue Resistance | |
| Springs | Mechanical Properties | High Strength | |
| Tooling for Mold Plastics | Conductivity (Electrical) | Electrical Conductivity | |
| Tooling for Mold Plastics | Corrosion Resistance | Corrosion Resistance | |
| Tooling for Mold Plastics | Creep Properties | Creep Resistant | |
| Tooling for Mold Plastics | Friction & Wear Properties | Wear Resistance | |
| Tooling for Mold Plastics | Mechanical Properties | High Strength | |
| Tooling for Mold Plastics | Softening Resistance | Resistance to Thermal Softening | |
| Wire | Conductivity (Electrical) | Electrical Conductivity | |
| Wire | Conductivity (Thermal) | Thermal Conductivity | |
| Wire | Corrosion Resistance | Corrosion Resistance | |
| Wire | Mechanical Properties | High Strength |
| Form | Specific Sub-Form | Application | System | Standard | Description |
|---|---|---|---|---|---|
| Sheet | ASTM | B768 | COPPER-COBALT-BERYLLIUM ALLOY SHEET AND STRIP | ||
| Strip | ASTM | B888/B88M | COPPER ALLOY STRIP FOR USE IN MANUFACTURE OF ELECTRICAL CONNECTORS OR SPRING CONTACTS | ||
| ASTM | B768 | COPPER-COBALT-BERYLLIUM ALLOY SHEET AND STRIP |
Corrosion Properties