Find suppliers for this alloy
C17455
| Elements | |||||||||
|---|---|---|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Sn | Fe | Ni(3) | Al | Be | Si | Zr | |
|
(1) Cu + Sum of Named Elements 99.5% min. (2) Cu value includes Ag. (3) Ni value includes Co. |
|||||||||
| Min (%) | 0.20 | 0.50 | 0.15 | ||||||
| Max (%) | Rem | 0.6 | 0.25 | 0.20 | 1.0 | 0.20 | 0.50 | 0.20 | 0.50 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.2% Offset (ksi) |
Elongation (%) |
Rockwell B scale |
|---|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | ||||||
| Rod | 1/2 Hard and Precipitation Heat Treated | TH02 |
100 Typ |
85 Typ |
15 Min |
93 Typ |
| Wire | 1/2 Hard and Precipitation Heat Treated | TH02 |
100 Typ |
85 Typ |
15 Min |
93 Typ |
| Melting Point - Liquidus°F | 1960 |
|---|---|
| Melting Point - Solidus°F | 1885 |
| Densitylb/cu in. at 68°F | 0.323 |
| Specific Gravity | 8.94 |
| Electrical Conductivity% IACS at 68°F | 52 |
| Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F | 128 |
| Modulus of Elasticity in Tensionksi | 20000 |
| Technique | Suitability |
|---|---|
| Soldering | Good |
| Brazing | Good |
| Oxyacetylene Welding | Not Recommended |
| Gas Shielded Arc Welding | Fair |
| Coated Metal Arc Welding | Fair |
| Spot Weld | Good |
| Seam Weld | Fair |
| Butt Weld | Fair |
| Capacity for Being Cold Worked | Excellent |
| Capacity for Being Hot Formed | Excellent |
Common Fabrication Processes
| Treatment | Minimum* | Maximum* | Medium | |
|---|---|---|---|---|
| * Temperature is measured in Fahrenheit. | ||||
| Hot Working Temperature | 1200 | 1750 | ||
| Solution Treatment | 1550 | 1700 | Air | |
Typical Uses