Chemical Composition
Element
Cu(1,2)FeNi(3)CrSi
(1) Cu + Sum of Named Elements 99.5% min. (2) Cu value includes Ag. (3) Ni value includes Co.
Min (%)1.80.100.40
Max (%)Rem0.153.00.80.8
Mechanical Properties

No mechanical properties for this alloy

Physical Properties

No physical properties for this alloy

Fabrication Properties

No fabrication properties for this alloy

Fabrication Process Properties

No fabrication process properties for this alloy

Thermal Characteristics

No thermal characteristics for this alloy

Typical uses
Product Category Product Reason Category Reason
IndustrialBlow Pins, Pinch Offs, Mold Cavities for Bold MoldsConductivity (Thermal)Thermal Conductivity
Blow Pins, Pinch Offs, Mold Cavities for Bold MoldsCorrosion ResistanceCorrosion Resistance
Blow Pins, Pinch Offs, Mold Cavities for Bold MoldsCorrosion ResistanceCorrosion Resistance to PVC
Blow Pins, Pinch Offs, Mold Cavities for Bold MoldsFinishing CharacteristicsAccepts High Surface Finishes
Blow Pins, Pinch Offs, Mold Cavities for Bold MoldsFriction & Wear PropertiesWear Resistance
Blow Pins, Pinch Offs, Mold Cavities for Bold MoldsMachining CharacteristicsMachinability
Blow Pins, Pinch Offs, Mold Cavities for Bold MoldsMechanical PropertiesHigh Strength
Cores, Core & Ejector Pins for Injection MoldsConductivity (Thermal)Thermal Conductivity
Cores, Core & Ejector Pins for Injection MoldsCorrosion ResistanceCorrosion Resistance
Cores, Core & Ejector Pins for Injection MoldsCorrosion ResistanceCorrosion Resistance to PVC
Cores, Core & Ejector Pins for Injection MoldsFinishing CharacteristicsAccepts High Surface Finishes
Cores, Core & Ejector Pins for Injection MoldsFriction & Wear PropertiesWear Resistance
Cores, Core & Ejector Pins for Injection MoldsMachining CharacteristicsMachinability
Cores, Core & Ejector Pins for Injection MoldsMechanical PropertiesHigh Strength
Heat Sink Inserts in Steel Plastic MoldsConductivity (Thermal)Thermal Conductivity
Heat Sink Inserts in Steel Plastic MoldsCorrosion ResistanceCorrosion Resistance
Heat Sink Inserts in Steel Plastic MoldsMachining CharacteristicsMachinability
Heat Sink Inserts in Steel Plastic MoldsMechanical PropertiesHigh Strength
Hot Runner Systems for Injection MoldsConductivity (Thermal)Thermal Conductivity
Hot Runner Systems for Injection MoldsCorrosion ResistanceCorrosion Resistance
Hot Runner Systems for Injection MoldsCorrosion ResistanceCorrosion Resistance to PVC
Hot Runner Systems for Injection MoldsFinishing CharacteristicsAccepts High Surface Finishes
Hot Runner Systems for Injection MoldsFriction & Wear PropertiesWear Resistance
Hot Runner Systems for Injection MoldsMachining CharacteristicsMachinability
Plunger Tips for Metal Die Casting MachinesBearing PropertiesLow Friction and Wear When Run Against Steel
Plunger Tips for Metal Die Casting MachinesConductivity (Thermal)High Thermal Conductivity
Plunger Tips for Metal Die Casting MachinesCorrosion ResistanceCorrosion Resistance
Plunger Tips for Metal Die Casting MachinesMechanical PropertiesHigh Strength
Resistance Welding TipsConductivity (Electrical)Electrical Conductivity
Resistance Welding TipsConductivity (Thermal)Thermal Conductivity
Resistance Welding TipsSoftening ResistanceResistance to Thermal Softening
Resistance Welding Wheels and FixturesConductivity (Electrical)Electrical Conductivity
Resistance Welding Wheels and FixturesConductivity (Thermal)Thermal Conductivity
Resistance Welding Wheels and FixturesCorrosion ResistanceCorrosion Resistance
Resistance Welding Wheels and FixturesCreep PropertiesCreep Resistant
Resistance Welding Wheels and FixturesMechanical PropertiesHigh Strength
Resistance Welding Wheels and FixturesSoftening ResistanceResistance to Thermal Softening
Sprue Bushing, Cavities for Injection MoldsConductivity (Thermal)Thermal Conductivity
Sprue Bushing, Cavities for Injection MoldsCorrosion ResistanceCorrosion Resistance
Sprue Bushing, Cavities for Injection MoldsCorrosion ResistanceCorrosion Resistance to PVC
Sprue Bushing, Cavities for Injection MoldsFinishing CharacteristicsAccepts High Surface Finishes
Sprue Bushing, Cavities for Injection MoldsFriction & Wear PropertiesWear Resistance
Sprue Bushing, Cavities for Injection MoldsMachining CharacteristicsMachinability
Stud Welding Collets and TipsConductivity (Electrical)Electrical Conductivity
Stud Welding Collets and TipsConductivity (Thermal)Thermal Conductivity
Stud Welding Collets and TipsCorrosion ResistanceCorrosion Resistance
Stud Welding Collets and TipsCreep PropertiesCreep Resistant
Stud Welding Collets and TipsMechanical PropertiesHigh Strength
Stud Welding Collets and TipsSoftening ResistanceResistance to Thermal Softening
Welding Dies for Wire and FlashConductivity (Electrical)Electrical Conductivity
Welding Dies for Wire and FlashConductivity (Thermal)Thermal Conductivity
Welding Dies for Wire and FlashCorrosion ResistanceCorrosion Resistance
Welding Dies for Wire and FlashCorrosion ResistanceDezincification Resistance
Welding Dies for Wire and FlashMechanical PropertiesHigh Strength
Applicable Specifications

No applicable specifications for this alloy

Corrosion Properties

No information available.