| Elements | |||||
|---|---|---|---|---|---|
| Cu(1,2) | Sn | Zn | P | Cr | |
|
(1) Includes oxygen-free or deoxidized grades with deoxidizers (such as phosphorus boron lithium or others in an amount agreed upon. (2) Cu value includes Ag. |
|||||
| Min (%) | 0.20 | 0.05 | 0.005 | 0.25 | |
| Max (%) | Rem | 0.30 | 0.15 | 0.015 | 0.35 |