Find suppliers for this alloy
C18142
| Elements | |||
|---|---|---|---|
| Cu(1,2) | Cr | Mg | |
|
(1) Cu + Sum of Named Elements 99.5% min. (2) Includes Ag. |
|||
| Min (%) | 0.20 | 0.05 | |
| Max (%) | Rem | 0.30 | 0.30 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.2% Offset (ksi) |
Elongation (%) |
Vickers Hardness, 3000 gm |
|---|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | ||||||
| Sheet & Strip | Hard | H04 |
73 Min 80 Typ 87 Max |
68 Min 77 Typ 86 Max |
10 Typ |
170 Typ |
| Melting Point - Liquidus°F | 1981 |
|---|---|
| Melting Point - Solidus°F | 1980 |
| Densitylb/cu in. at 68°F | 0.32 |
| Specific Gravity | 8.9 |
| Electrical Conductivity% IACS at 68°F | 80 |
| Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F | 191 |
| Coefficient of Thermal Expansion 68-57210 to -6 power per °F (68 – 572°F) | 17 |
| Modulus of Elasticity in Tensionksi | 20300 |
| Poisson's Ratio | 0.33 |
| Technique | Suitability |
|---|---|
| Soldering | Good |
| Capacity for Being Cold Worked | Good |
| Capacity for Being Hot Formed | Good |
Common Fabrication Processes
- Bending
- Cold working
- Stamping
Thermal Properties
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Electrical | Connectors, Electrical, Lead-Free | ||
| Electrical and electronic terminals, connectors, Lead frames |
Applicable Specifications
Corrosion Properties