Find suppliers for this alloy
C18550
| Elements | |||
|---|---|---|---|
| Cu(1) | Sn | Cr | |
|
(1) Cu value includes Ag. |
|||
| Min (%) | 0.10 | 0.6 | |
| Max (%) | Rem | 0.14 | 1.0 |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties