C18910
| Elements | ||||
|---|---|---|---|---|
| Cu(1) | P | Mn | Si | |
|
(1) Cu value includes Ag. |
||||
| Min (%) | ||||
| Max (%) | Rem | 0.15 | 0.50 | 0.50 |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties