C18990
| Elements | ||||
|---|---|---|---|---|
| Cu(1,2) | Sn | P | Cr | |
|
(1) Cu + Sum of Named Elements 99.9% min. (2) Cu value includes Ag. |
||||
| Min (%) | 1.8 | 0.005 | 0.10 | |
| Max (%) | Rem | 2.2 | 0.015 | 0.20 |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Industrial | Welding Wire | Conductivity (Electrical) | Electrical Conductivity |
| Welding Wire | Conductivity (Thermal) | Thermal Conductivity | |
| Welding Wire | Softening Resistance | Resistance to Thermal Softening |
Applicable Specifications
Corrosion Properties