C19020
| Elements | ||||
|---|---|---|---|---|
| Cu(1,2) | Sn | P | Ni | |
|
(1) Cu + Sum of Named Elements 99.8% min. (2) Cu value includes Ag. |
||||
| Min (%) | 0.30 | 0.01 | 0.50 | |
| Max (%) | Rem | 0.9 | 0.20 | 3.0 |