Find suppliers for this alloy
C19022
| Elements | |||||||
|---|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Sn | Zn | Fe | P | Ni(3) | |
|
(1) Cu + Sum of Named Elements 99.5% min. (2) Cu value includes Ag. (3) Ni value includes Co. |
|||||||
| Min (%) | 0.3 | 0.01 | 0.3 | ||||
| Max (%) | Rem | 0.009 | 1.0 | 0.2 | 0.04 | 0.07 | 1.0 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.2% Offset (ksi) |
Elongation (%) |
Vickers Hardness, 500 gm |
|---|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | ||||||
| Strip | Annealed Tempers, O | O |
40 Typ |
15 Typ |
40 Typ |
60 Min |
| Melting Point - Liquidus°F | 1976 |
|---|---|
| Melting Point - Solidus°F | 1926 |
| Densitylb/cu in. at 68°F | 0.32 |
| Specific Gravity | 8.9 |
| Electrical Conductivity% IACS at 68°F | 48 |
| Coefficient of Thermal Expansion 68-21210 to -6 power per °F (68 – 212°F) | 9.4 |
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties