Find suppliers for this alloy
C19030
| Elements | ||||||
|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Sn | Fe | P | Ni | |
|
(1) Cu value includes Ag. (2) Cu + Sum of Named Elements 99.7% min. |
||||||
| Min (%) | 1.0 | 0.01 | 1.5 | |||
| Max (%) | Rem | 0.02 | 1.5 | 0.10 | 0.03 | 2.0 |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties