Find suppliers for this alloy
C19150
Elements | ||||||
---|---|---|---|---|---|---|
Cu(1,2) | Pb | Sn | Fe | P | Ni | |
(1) Cu + Sum of Named Elements 99.5% min. (2) Cu value includes Ag. |
||||||
Min (%) | 0.50 | 0.15 | 0.8 | |||
Max (%) | Rem | 1.0 | 0.05 | 0.05 | 0.35 | 1.2 |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Product Category | Product | Reason Category | Reason |
---|---|---|---|
Electrical | Contacts | Conductivity (Electrical) | Electrical Conductivity |
Contacts | Conductivity (Thermal) | Thermal Conductivity | |
Contacts | Corrosion Resistance | Corrosion Resistance | |
Contacts | Mechanical Properties | Moderate Strength | |
Contacts | Solderability | Solderability |
Applicable Specifications
Corrosion Properties