Find suppliers for this alloyC19210
Chemical Composition
Element
Cu(1)FeP
(1) Cu + Sum of Named Elements 99.8% min.
Min (%)0.050.025
Max (%)Rem0.150.04
Mechanical Properties*
Form
Temper
Temper Code
Tensile Strength
(ksi)
YS-0.2% Offset
Elongation
(%)
Section Size
(in)
Sheet1/2 HardH0257   Typ
56   Typ
6   Typ
0.018
1/4 HardH0150   Typ
48   Typ
13   Typ
0.018
HardH0464   Typ
63   Typ
3.5   Typ
0.018
Light AnnealO5043   Typ
22   Typ
38   Typ
0.018
SpringH0871   Typ
70   Typ
2   Typ
0.018
* Measured at room temperature, 68°F (20°C).
Physical Properties
Melting Point - Liquidus°F1980
Densitylb/cu in. at 68°F0.323
Specific Gravity8.94
Electrical Conductivity% IACS at 68°F80
Coefficient of Thermal Expansion 68-57210⁻⁶ per °F (68 – 572°F)9.4
Specific Heat CapacityBtu/ lb /°F at 68°F0.092
Modulus of Elasticity in Tensionksi18200
Fabrication Properties
Technique Suitability
SolderingExcellent
BrazingExcellent
Oxyacetylene WeldingGood
Gas Shielded Arc WeldingNot Recommended
Coated Metal Arc WeldingExcellent
Spot WeldNot Recommended
Seam WeldNot Recommended
Butt WeldGood
Capacity for Being Cold WorkedExcellent
Capacity for Being Hot FormedExcellent
Forgeability Rating65
Machinability Rating20
Common Fabrication Processes
  • Forming and Bending
  • Heading and Upsetting
  • Piercing and Punching
  • Shearing
  • Spinning
  • Squeezing and Swaging
  • Stamping
    
Thermal Properties
Treatment Minimum* Maximum*
* Temperature is measured in Fahrenheit.
Annealing8401020
Hot Treatment13001650
Typical uses
Product Category Product Reason Category Reason
AutomotiveCooling Fins for RadiatorsConductivity (Thermal)Thermal Conductivity
Cooling Fins for RadiatorsCorrosion ResistanceCorrosion Resistance
Cooling Fins for RadiatorsForming CharacteristicsFormability
Cooling Fins for RadiatorsMechanical PropertiesModerate Strength
BuildingAir Conditioning TubingCorrosion ResistanceCorrosion Resistance
Air Conditioning TubingMechanical PropertiesModerate Strength
Air Conditioning TubingSolderabilitySolderability
Air Conditioning TubingWelding CharacteristicsWeldability
ElectricalConnectorsConductivity (Electrical)Electrical Conductivity
ConnectorsConductivity (Thermal)Thermal Conductivity
ConnectorsCorrosion ResistanceCorrosion Resistance
ConnectorsMechanical PropertiesModerate Strength
IC Lead FramesConductivity (Electrical)Electrical Conductivity
IC Lead FramesConductivity (Thermal)Thermal Conductivity
IC Lead FramesCorrosion ResistanceCorrosion Resistance
IC Lead FramesForming CharacteristicsFormability
IC Lead FramesMechanical PropertiesModerate Strength
IC Lead FramesSolderabilitySolderability
TerminalsConductivity (Electrical)Electrical Conductivity
TerminalsConductivity (Thermal)Thermal Conductivity
TerminalsCorrosion ResistanceCorrosion Resistance
TerminalsForming CharacteristicsFormability
TerminalsMechanical PropertiesModerate Strength
TerminalsSolderabilitySolderability
IndustrialCooling Fins for Heavy Duty RadiatorsConductivity (Thermal)Thermal Conductivity
Cooling Fins for Heavy Duty RadiatorsCorrosion ResistanceCorrosion Resistance
Cooling Fins for Heavy Duty RadiatorsForming CharacteristicsFormability
Cooling Fins for Heavy Duty RadiatorsMechanical PropertiesModerate Strength
Cooling Fins for Heavy Duty RadiatorsSoftening ResistanceResistance to Thermal Softening
Heat Exchanger TubingAppearanceAppearance
Heat Exchanger TubingConductivity (Thermal)Thermal Conductivity
Heat Exchanger TubingCorrosion ResistanceCorrosion Resistance
Heat Exchanger TubingForming CharacteristicsFormability
Heat Exchanger TubingMechanical PropertiesModerate Strength
Heat Resistant ApplicationsConductivity (Thermal)Thermal Conductivity
Heat Resistant ApplicationsCorrosion ResistanceCorrosion Resistance
Heat Resistant ApplicationsForming CharacteristicsFormability
Heat Resistant ApplicationsMechanical PropertiesModerate Strength
Applicable Specifications
Form Specific Sub-Form System Standard Description
StripElectric Connector & Spring ContactASTMB888/B88MCOPPER ALLOY STRIP FOR USE IN MANUFACTURE OF ELECTRICAL CONNECTORS OR SPRING CONTACTS
Strip, Sheet & PlateASTMB465COPPER-IRON ALLOY PLATE, SHEET, STRIP, AND ROLLED BAR
Corrosion Properties