C19260
| Elements | ||||
|---|---|---|---|---|
| Cu(1) | Fe | Mg | Ti | |
|
(1) Cu + Sum of Named Elements 99.9% min. |
||||
| Min (%) | 98.5 | 0.40 | 0.02 | 0.20 |
| Max (%) | 0.8 | 0.15 | 0.40 | |