Find suppliers for this alloy
C19520
| Elements | |||
|---|---|---|---|
| Cu(1) | Pb | Fe | |
|
(1) Cu + Sum of Named Elements 99.8% min. |
|||
| Min (%) | 96.6 | 0.01 | 0.50 |
| Max (%) | 3.5 | 1.5 | |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Electrical | Lead Frames | Conductivity (Electrical) | Electrical Conductivity |
| Lead Frames | Conductivity (Thermal) | Thermal Conductivity | |
| Lead Frames | Corrosion Resistance | Corrosion Resistance | |
| Lead Frames | Mechanical Properties | High Strength | |
| Lead Frames | Solderability | Solderability |
Applicable Specifications
Corrosion Properties