Chemical Composition
Element
CuZnFeP
Min (%)0.90.25
Max (%)Rem0.351.20.35
Mechanical Properties

No mechanical properties for this alloy

Physical Properties
Densitylb/cu in. at 68°F0.32
Specific Gravity8.86