Find suppliers for this alloyC19700
Chemical Composition
Element
Cu(1)PbSnZnFePNiCoMgMn
(1) Cu + Sum of Named Elements 99.8% min.
Min (%)0.300.100.01
Max (%)Rem0.050.200.201.20.400.050.050.200.05
Mechanical Properties

No mechanical properties for this alloy

Physical Properties
Densitylb/cu in. at 68°F0.319
Specific Gravity8.83
Fabrication Properties

No fabrication properties for this alloy

Fabrication Process Properties

No fabrication process properties for this alloy

Thermal Characteristics

No thermal characteristics for this alloy

Typical uses
Product Category Product Reason Category Reason
ElectricalCable ShieldingConductivity (Thermal)Thermal Conductivity
Cable ShieldingCorrosion ResistanceCorrosion Resistance
Cable ShieldingForming CharacteristicsFormability
Cable ShieldingSoftening ResistanceResistance to Thermal Softening
Circuit Breaker ComponentsConductivity (Electrical)Electrical Conductivity
Circuit Breaker ComponentsConductivity (Thermal)Thermal Conductivity
Circuit Breaker ComponentsCorrosion ResistanceCorrosion Resistance
Circuit Breaker ComponentsForming CharacteristicsFormability
Circuit Breaker ComponentsMechanical PropertiesHigh Strength
ConnectorsConductivity (Electrical)Electrical Conductivity
ConnectorsConductivity (Thermal)Thermal Conductivity
ConnectorsCorrosion ResistanceCorrosion Resistance
ConnectorsMechanical PropertiesHigh Strength
Fuse ClipsConductivity (Electrical)Electrical Conductivity
Fuse ClipsConductivity (Thermal)Thermal Conductivity
Fuse ClipsCorrosion ResistanceCorrosion Resistance
Fuse ClipsForming CharacteristicsFormability
Fuse ClipsMechanical PropertiesHigh Strength
Lead FramesConductivity (Electrical)Electrical Conductivity
Lead FramesConductivity (Thermal)Thermal Conductivity
Lead FramesCorrosion ResistanceCorrosion Resistance
Lead FramesMechanical PropertiesHigh Strength
Lead FramesSolderabilitySolderability
Applicable Specifications
Form Specific Sub-Form System Standard Description
BarASTMB465COPPER-IRON ALLOY PLATE, SHEET, STRIP, AND ROLLED BAR
PlateASTMB465COPPER-IRON ALLOY PLATE, SHEET, STRIP, AND ROLLED BAR
SheetASTMB465COPPER-IRON ALLOY PLATE, SHEET, STRIP, AND ROLLED BAR
StripASTMB465COPPER-IRON ALLOY PLATE, SHEET, STRIP, AND ROLLED BAR
Electric Connector & Spring ContactASTMB888/B88MCOPPER ALLOY STRIP FOR USE IN MANUFACTURE OF ELECTRICAL CONNECTORS OR SPRING CONTACTS
Corrosion Properties

No information available.