| Elements | ||||||||||
|---|---|---|---|---|---|---|---|---|---|---|
| Cu(1) | Pb | Sn | Zn | Fe | P | Ni | Co | Mg | Mn | |
|
(1) Cu + Sum of Named Elements 99.8% min. |
||||||||||
| Min (%) | 0.05 | 0.35 | 0.10 | 0.01 | ||||||
| Max (%) | Rem | 0.05 | 0.40 | 0.20 | 1.2 | 0.40 | 0.05 | 0.05 | 0.20 | 0.05 |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties